由于很多职业在应用保温铝卷时,对其平整度要求较高,所以铝卷生产厂家对保温铝卷这一出产环节的把控分外谨慎。下面厂家为您解说一番。
Because many professions have high requirements for flatness when applying thermal insulation aluminum coils, the aluminum coil manufacturers are extremely cautious in controlling the production process of thermal insulation aluminum coils. The manufacturer will explain it to you.
1、使用修模来改善保温铝卷的平整度
1. Use mold repair to improve the flatness of thermal insulation aluminum coil
修模是国内外关于揉捏材平整度不良常用的解决方法,保温铝卷的平面空隙不良,主要是和模具的流速不均有关,经过改动导流槽的巨细或视点,再或是改动工作带的长短来有用的调整金属流速,以便流速均匀,消除平面空隙不良的缺陷。
Mold repair is a common solution to the poor flatness of kneaded materials at home and abroad. The poor plane clearance of thermal insulation aluminum coil is mainly related to the uneven flow rate of the mold. The metal flow rate can be effectively adjusted by changing the size or view point of the guide groove or the length of the working belt, so that the flow rate is uniform and the defects of poor plane clearance can be eliminated.
2、使用离线精整来批改保温铝卷平整度
2. Use offline finishing to correct the flatness of thermal insulation aluminum coil
先根据保温铝卷具体平整度超差的特征,合理装备离线精整机的辊片,然后选用一只平整度超差的制品进行定辊,经过不断调整辊片的高度和方位,待该只保温铝卷的平面度合格后,固定辊片的高度和方位,然后对该批次的制品进行离线精整。
First, according to the characteristics of the specific flatness of the thermal insulation aluminum coil, reasonably equip the roll sheet of the offline finishing machine, and then select a product with flatness out of tolerance to fix the roll. After continuously adjusting the height and orientation of the roll sheet, after the flatness of the thermal insulation aluminum coil is qualified, fix the height and orientation of the roll sheet, and then conduct offline finishing for the products of this batch.
3、选用在线精整来批改保温铝卷平整度
3. Select online finishing to correct the flatness of thermal insulation aluminum coil
在线精整是根据离线精整的原理,在原揉捏机出口导正装置的基础上加装轴承座及辊片,经过调节辊片的高度和方位来改动对保温铝卷压力的巨细使其发作一定量的变形,让保温铝卷的平整度控制在合理的范围内,然后到达在线精整的意图。
On line finishing is based on the principle of offline finishing, the bearing seat and roll sheet are added on the basis of the original kneading machine outlet guide device. The height and orientation of the roll sheet are adjusted to change the size of the pressure on the aluminum insulation coil, so that it has a certain amount of deformation, so that the flatness of the aluminum insulation coil is controlled within a reasonable range, and then the intention of online finishing is reached.