澳门生肖号码表
当前位置:首页-新闻资讯

加工铝材时遇到的问题

来源:/ 发布时间:2022-11-26

加工纯铝时,容易粘刀的几点分析是怎样的呢?下面铝板生产厂家为您讲解一番。
When processing pure aluminum, what is the analysis of the easy sticking of the knife? Next, the aluminum plate manufacturer will explain it to you.
1、铝材料质地偏软高温容易粘刀;
1. The aluminum material is soft and easy to stick the knife at high temperature;
2、铝不耐高温,容易开纹;
2. Aluminum is not resistant to high temperature and easy to crack;
3、跟加工切削液有关:油性润滑性能好;水溶性冷却性能好;干切削费用高;
3. It is related to the cutting fluid: good oil lubrication performance; Good water soluble cooling performance; High cost of dry cutting;
4、加工纯铝时,应选用铝加工专用的立铣刀:正前角,刃口锋利,大排屑槽,45度或55度的螺旋角;
4. When processing pure aluminum, the end milling cutter specially used for aluminum processing shall be selected: positive front angle, sharp edge, large chip discharge groove, 45 ° or 55 ° spiral angle;

铝板生产厂家
5、被加工件和数控刀具的材料具有较大的亲和力。
5. The materials of machined parts and NC tools have a greater affinity.
6、前刀面粗糙刀具加工软的材料。建议:机床条件差到好要求低到高,请分别使用高速钢,涂层抛光硬质合金、PCD聚晶金刚石和单晶金刚石。
6. Rough rake face tools process soft materials. Suggestion: The machine tool conditions are poor to good, and the requirements are low to high. Please use high-speed steel, coated and polished cemented carbide, PCD polycrystalline diamond and single crystal diamond respectively.
7、速度低可用切削液避免,速度高用油雾润滑,效果可改善。
7. Low speed can be avoided with cutting fluid, high speed can be lubricated with oil mist, and the effect can be improved.
加工铝材时遇到的问题相关内容就讲解到这里了,您对此有什么想咨的问题欢迎来我们网站咨询了解!
So much for the problems encountered in aluminum processing. If you have any questions, please come to our website Ask about it!